As above, what is the best way to heat PCL pellets to make them soft enough for sculpting.
I’d like to avoid anything that includes a naked flame as I also use a lot of alcohol based chemicals, so there is a fire risk.
As above, what is the best way to heat PCL pellets to make them soft enough for sculpting.
I’d like to avoid anything that includes a naked flame as I also use a lot of alcohol based chemicals, so there is a fire risk.
Glass/Melt temperature is ~60C.
Afik most people modelling with this just use hot water, I’ve never done it myself but seen videos of it being done. Assuming you have a kettle or electric water heater you will be fine, I imagine you could use hot air from a hairdryer or similar too. But water seems to be the usual method.